Audio & Video Tech General discussion of audio and video for the Ford Ranger.

help fiberglassing

Old May 13, 2007
  #1  
greenmonster98's Avatar
Thread Starter
|
Member
Joined: Feb 2007
Posts: 56
Likes: 0
From: Washougal, WA
help fiberglassing

I am done constructing the frame of my box and have laid 2 layers of fiberglass. I think I am going to put on 1 or 2 more layers. What do I do after laying the fiberglass? Do I just start putting on the body filler? I bought some short stranded fiberglass filler and some Rage Gold,but im not really sure what the difference is?
 
Reply
Old May 13, 2007
  #2  
2003stealthedge's Avatar
Joined: May 2005
Posts: 1,297
Likes: 0
From: The ILL State
i didnt see anything on you laying the fleece around the box make sure you did that. Lay about 5-6 layers of glass on there let dry for a good 12-24 hours then bondo it or use rage gold. Then sand. This is the part thats gonna take AWHILE sanding a box to perfection is a PITA. Goto an autobody supply store and grab some grrr whats it called, the stuff the use to fill bondo i cant think of the name of it.
 
Reply
Old May 13, 2007
  #3  
HighRollerII's Avatar
RF Veteran
iTrader: (4)
Joined: Jun 2004
Posts: 10,073
Likes: 4
From: Charleston, SC
high build primer will also be your best friend..
 
Reply
Old May 13, 2007
  #4  
greenmonster98's Avatar
Thread Starter
|
Member
Joined: Feb 2007
Posts: 56
Likes: 0
From: Washougal, WA
what do you mean lay the fleace down? I streched some spandex like material over the box, put some resin on it, and when that dryed I started laying fiberglass.
 
Reply
Old May 13, 2007
  #5  
greenmonster98's Avatar
Thread Starter
|
Member
Joined: Feb 2007
Posts: 56
Likes: 0
From: Washougal, WA
I ran out of resin after the second layer of FG. Is it ok to start fiberglassing over it again tomorrow? My only option is to pick up more resin tomorrow and continue.
 
Reply
Old May 13, 2007
  #6  
2003stealthedge's Avatar
Joined: May 2005
Posts: 1,297
Likes: 0
From: The ILL State
spandex wont hold alot of resin. You need fleece or some kind of cotton because itll absorb alot of resin. That spandex stuff is most likely thin and the resin wont hold onto it well even though it may seem. Id goto like a fabric store and get some fleece and re wrap it so its stronger and seals better
 
Reply
Old May 13, 2007
  #7  
Lone-Ranger's Avatar
Member
Joined: May 2006
Posts: 201
Likes: 0
From: Tri-Cities
well what you use for the base material really dosnt matter a whole lot after you get the fiberglass down. Yes, its fine to start back up on laying glass tomorrow, and i would get atleast 5-6 layers down before you continue. After you have let the glass fully cure i take that short strand reinforced filler and lay a nice layer over the entire glass surface. Once that cures grind it down to get close to the final profile. By then you should have a surface that is very close to what you want. Mix up some rage and add enough resin to it to make it like a thick soup. Spread this mixture over the entire thing and then try and sand as much as you can in the green stage. I generally do this one more time then hit it with bondo pinhole filler. From there it is primer, sand primer,sand, primer, sand, as much as it takes. Good luck and lets see some pics.
 
Reply
Old May 14, 2007
  #8  
greenmonster98's Avatar
Thread Starter
|
Member
Joined: Feb 2007
Posts: 56
Likes: 0
From: Washougal, WA
i based it off of the design that Lone Ranger made. I looks pretty good right now. I have 5 coats on right now and I think tomorrow i will start with the short strand stuff. I had to modify it because my seats come out of the side of the x cab. SO i made a piece to cover the opening. Thanks for all the help. Ill post pics when I get my camera. thanks for all the help guys. Especially Lone Ranger he knows his stuff.

thanks
 
Reply
Old Jun 24, 2007
  #9  
ranger riden high's Avatar
Joined: Jun 2007
Posts: 19
Likes: 0
From: dallas,ga
heres a great place to look for ideas,tricks of the trade, or anything to do with fiberglasing.
Thanks to this website i bring in around $600 a weekend making boxes for ppl. im only 16
Good luck buddy!
http://www.the12volt.com/installbay/...ics.asp~FID~16
 
Reply
Old Jun 28, 2007
  #10  
someonelazy's Avatar
Member
Joined: Jun 2007
Posts: 53
Likes: 0
From: Mesa, Arizona
Originally Posted by 2003stealthedge
i didnt see anything on you laying the fleece around the box make sure you did that. Lay about 5-6 layers of glass on there let dry for a good 12-24 hours then bondo it or use rage gold. Then sand. This is the part thats gonna take AWHILE sanding a box to perfection is a PITA. Goto an autobody supply store and grab some grrr whats it called, the stuff the use to fill bondo i cant think of the name of it.
i believe your thinking of a glaze coat, ive had best experiance/easy sanding with evercoat, its pricey, but gets the job done.
 
Reply
Related Topics
Thread
Thread Starter
Forum
Replies
Last Post
EdGe_wannabe
Exterior Semi-Tech
10
Jun 2, 2007 01:28 PM
Sychodemeanor
Audio & Video Tech
23
Mar 30, 2006 01:17 AM
advantEDGE
Interior Semi-Tech
37
Aug 20, 2005 10:09 AM
Skyjacker_44
Interior Semi-Tech
2
Jan 16, 2005 07:20 AM


Thread Tools
Search this Thread

All times are GMT -6. The time now is 04:20 PM.